Raw material bamboo charcoal obtained by firing a bamboo material is refired at 500 to 1,200°C for 5 to 11 hr.例文帳に追加
竹材を焼成してなる原料竹炭を、さらに、500〜1200℃で5〜11時間かけて再焼成する。 - 特許庁
A granulated material for road pavement material for pedestrian is prepared by containing 10-50 wt.% cement in completely incinerated ash refired under a high temp. atmosphere and the road pavement material for pedestrian is obtained by mixing coarse sand and a cement-based hardening agent with the granulated material.例文帳に追加
本発明の歩行者系道路舗装用造粒物は、高温雰囲気で再燃焼した完全焼却灰にセメント10〜50重量%を含有したものであり、この造粒物は、粗目砂及びセメント系固化材を混合して歩行者系道路舗装材を得る。 - 特許庁
In the method where ammonium hexachlororuthenate ((NH_4)_3RuCl_6) is fired, so as to produce ruthenium powder, ammonium hexachlororuthenate is fired at 500 to 800°C to obtain crude ruthenium, and the crude ruthenium is pulverized and is thereafter refired at 800 to 1,000°C, thus the content of chlorine in the ruthenium powder is controlled to ≤100 mass ppm.例文帳に追加
ヘキサクロロルテニウム酸アンモニウム((NH_4)_3RuCl_6)を焼成してルテニウム粉末を製造する工程において、ヘキサクロロルテニウム酸アンモニウムを500〜800℃で焼成して得た粗ルテニウムを粉砕後、800〜1000℃で再焼成することにより、ルテニウム粉末中の塩素含有量が100mass ppm以下であるルテニウム粉末を製造する方法。 - 特許庁