The flexible polyurethane foam having closed cells has an average cell diameter of 70 μm or less and an Askar F hardness of 80 or less.例文帳に追加
平均気泡径が70μm以下、かつアスカーF硬度が80以下である独立気泡軟質ポリウレタンフォームとする。 - 特許庁
The closed cell foamed body has 3.5-12 times of foaming ratio, 65-90 degree of Askar F hardness and ≤30% of compression set.例文帳に追加
独立気泡体の発泡倍率は3.5〜12倍、アスカーF硬度が65〜90度、圧縮永久歪は30%未満が好ましい。 - 特許庁
In the heat-dissipating sheet having a two-layer structure in which a thermal conductive material is bonded by a bonding agent, a hardness difference between the Askar C hardness of one layer and that of the other layer ranges from 21 to 50.例文帳に追加
熱伝導性材料を結合剤で結合させた2層構造の放熱シートであって、一方の層のアスカーC硬度と他方の層のアスカーC硬度の硬度差が21〜50であることを特徴とする。 - 特許庁
The paving material 10 is formed by mixing a urethane binder and the third component material as hard aggregate with rubber chips and molding the mixture, and its hardness is 70-90 points at a measured value by an Askar CS hardness meter.例文帳に追加
舗装材10は、ゴムチップに、ウレタン系等のバインダー及び硬質骨材である第3成分材料を混合し成形して形成され、その硬さが、アスカーCS硬度計による計測値で70〜90ポイントである。 - 特許庁
In a rubber composition having closed and/or open cells containing a diene rubber component as a main component, the ASKAR-C hardness of the cured rubber composition is set in the range of 20° to 60°, a fracture strength equal to 3.0 MPa or higher and a fracture elongation equal to 250% or higher.例文帳に追加
ジエン系ゴム成分を主成分とする独立又は/及び連続した気泡を有するゴム組成物であって、加硫後の前記ゴム組成物のASKAR−C硬度が20°〜60°、破断強度が3.0MPa以上、破断伸度が250%以上とする。 - 特許庁